Product Introduction

The pipeline fire-resistant tape is installed more quickly and easily, without the need for hooks, anchor bolts, or drilling holes inside the substrate. It is suitable for solutions such as looping in narrow spaces or hard to reach areas. It is suitable for most penetration size product applications, with thermal expansion, flexible application, simple cutting, waterproof, and long-lasting fire-resistant performance. The non replaceable fire-resistant tape effectively blocks the spread of fire, smoke, and steam, protecting life and property safety.

Scope of use

Concrete, brick, wood flooring, and gypsum board walls with a thickness of over 100mm for walls and floors

Product specifications

  • Size specifications 10 meters * 45 * 5mm
    5 rolls/box/20kg
    Belt shaped soft roll material
    Product weight
    Product appearance

Product performance

Apparent density

≤1.6×10³kg/m³

Acid resistance

≥ 3d, no swelling or cracking

Water resistance

≥ 3d, no swelling or cracking

Humidity resistance

≥ 360h, no cracking or powdering

Alkali resistance

≥ 3d, no swelling or cracking

Freeze thaw cycle resistance

≥ 15 times, without cracking or powdering

Fire integrity

The fire resistance integrity is ≥ 3h, and the cotton pad on the back of the test piece is not ignited, No continuous flames for 10 seconds or more have occurred

Fire resistance and thermal insulation

Fire resistance and thermal insulation of ≥ 3h, with any penetrating object blocked from the back end of the flame The maximum surface temperature rise at 25mm of the material is ≤ 180 C

Inspection report

Have

Installation instructions

  • Clean the opening The surface prepared for spraying fireproof gap sealing material should be cleaned of scattered debris, dust, oil stains, moisture, and wax.
  • Insert mineral wool According to the test report, insert a backing material of sufficient thickness (such as mineral wool).
  • Spraying of fireproof gap sealing materials Apply fireproof gap sealing material to the required thickness Meet the corresponding fire protection time limit and confirm that the fireproof gap sealing material is applied to the entire backing surface and 12.5mm around it.
  • Curing of fireproof gap sealing materials At 23 C a thickness of 3mm requires 5-7 days to fully cure. If necessary for maintenance, an identification plate can be installed next to the joint